Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 305 MPa @Thickness 3.00 mm |
44200 psi @Thickness 0.118 in |
LT Direction |
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f.. |
|||
Compressive Strength | 305 MPa @Thickness 3.00 mm |
44200 psi @Thickness 0.118 in |
L Direction |
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f.. |