Polymer Property : Compressive Strength = 4410 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 30.4 MPa

@Temperature 1450 °C,
Time 7200 sec
4410 psi

@Temperature 2640 °F,
Time 2.00 hour
Cold Crushing Strength
Chosun Refractories AU3 Blast Furnace Runner Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).