Mechanical Properties Metric English Comments
Compressive Strength 262 MPa

@Temperature 260 °C
38000 psi

@Temperature 500 °F
Dry; 325°F Autoclave Cured; ASTM D695
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Compressive Strength 262 MPa

@Temperature 288 °C
38000 psi

@Temperature 550 °F
Wet; ASTM D6641
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric
MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-..
Compressive Strength 262 MPa

@Temperature 204 °C
38000 psi

@Temperature 400 °F
Open Hole, Wet; ASTM D7028
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin IM7 12K Carbon Uni-tape
Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures ..
Compressive Strength 262 MPa

@Temperature 177 °C
38000 psi

@Temperature 350 °F
Open Hole, Wet; ASTM D7028
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin IM7 12K Carbon Uni-tape
Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures ..