Polymer Property : Compressive Strength = 36.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 36.5 MPa

@Treatment Temp. 540 °C
5290 psi

@Treatment Temp. 1000 °F
Cold Crush Strength; Dried 104°C
BNZ Materials Blazecrete 3200 Dense Castable
Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special ..