Polymer Property : Compressive Strength = 36.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 36.0 MPa

@Strain 2 %
5220 psi

@Strain 2 %
ISO 604
Quadrant EPP Symalit® 1000 PVDF unfilled, extruded (ISO Data)
Symalit 1000 PVDF is a highly crystalline unreinforced fluoropolymer combining good mechanical, thermal and electrical properties with excellent chemical resistance. It also shows good resistance to..