Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 331 MPa @Temperature 23.9 °C |
48000 psi @Temperature 75.0 °F |
Dry; Oven Cure, 90min, 260°F; ASTM D695 |
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring .. |
|||
Compressive Strength | 331 MPa @Temperature 21.1 °C |
48000 psi @Temperature 70.0 °F |
Open Hole, Dry; ASTM D7028 |