Mechanical Properties Metric English Comments
Compressive Strength 317 MPa

@Temperature 23.9 °C
46000 psi

@Temperature 75.0 °F
Dry; 8HS form; ASTM D695
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, C2 Reinforced
Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel..
Compressive Strength 317 MPa

@Temperature 149 °C
46000 psi

@Temperature 300 °F
Wet; ASTM D695
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4503 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..