Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 20.7 MPa @Treatment Temp. 104 °C |
3000 psi @Treatment Temp. 219 °F |
Cold Crush Strength; Dried 104°C |
BNZ Materials Blazecrete 2800 Dense Castable Blazecrete 2800 is an economical, high alumina refractory for service to 2800°F (1556°C). Suitable for door linings, curbs and covers, pre-cast shapes, grey iron ladles, aluminum reverberatory fur.. |