Polymer Property : Compressive Strength = 270 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 1.86 MPa

@Temperature 1095 °C
270 psi

@Temperature 2003 °F
Cold Crush Strength
BNZ Materials Bazelite 2300 Insulating Castable
Blaz 2300 is a lightweight, general purpose insulating castable. Can be used for back-up or exposed to furnace conditions. Used for one-shot linings, petrochemical heaters, combustion chambers and f..