Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 18.5 MPa @Strain 2 % |
2680 psi @Strain 2 % |
ISO 604 |
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data) This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to.. |