Mechanical Properties Metric English Comments
Compressive Strength 2.34 MPa

@Temperature 1095 °C
340 psi

@Temperature 2003 °F
BNZ Materials Bazelite 2000 Insulating Castable
BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i..