Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 13.7 MPa @Temperature 110 °C |
1990 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics ZAP 013 Smart Cast Application Special Properties: Low Density, High Strength, Low Thermal ConductivityIndustry: Multi PurposeApplication: All type furnaces as a back up layer, Insulating Burner BlocksInformation provided by Shar.. |
|||
Compressive Strength | 13.7 MPa @Temperature 110 °C, Time 86400 sec |
1990 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories APC-50 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |