Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 125 MPa @Strain 2 % |
18100 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Ketron® CA30 PEEK + carbon fibres, extruded (ISO Data) This 30 % carbon fibre reinforced grade combines even higher stiffness, mechanical strength and creep resistance than Ketron PEEK-GF30 with an optimum wear resistance. Moreover, compared with unrein.. |
|||
Compressive Strength | 125 MPa @Temperature 23.0 °C |
18100 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
Compressive Strength | 125 MPa @Temperature 23.0 °C |
18100 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |