Compressive Strength 123 MPa

@Temperature 110 °C
17800 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics Smart Cast 9 Medium Cement Castables
Information provided by Sharadaa Ceramics Pvt. Ltd.