Polymer Property : Compressive Strength = 17700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 122 MPa

@Strain 5 %
17700 psi

@Strain 5 %
ISO 604
Quadrant EPP Techtron® PPS unfilled, extruded (ISO Data)
This unfilled polyphenylene sulfide based material is ideal for structural applications in corrosive environments or as a PEEK replacement at less demanding temperatures. Very good dimensional stabi..