Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 100 - 120 MPa @Temperature 1300 °C |
14500 - 17400 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 130 Dense Vibrating Refractory Castable Description: Vibron 130 is a vibrating castable with a low cement content, based on abrasion resistant spinel grains.Remarks: Indicated values apply to vibrated products.Information provided by Goud.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1300 °C |
14500 - 17400 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 Dense Vibrating Refractory Castable Description: Vibron 160 is a low cement vibrating castable on andalusite base, characterized by a high strength and excellent thermal shock resistance.Remarks: Indicated values apply to vibrated pro.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 H Dense Vibrating Refractory Castable Description: Vibron 160 H is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance.Remarks: Indicated values apply to vib.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 170 M Dense Vibrating Refractory Castable Description: Vibron 170 is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags.Remar.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 H RAPID Dense Vibrating Refractory Castable Description: Vibron 160 H Rap is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance. Because of special additives, thi.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 K Dense Vibrating Refractory Castable Description: Vibron 160 K is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity and high abrasion resistance. The thermal shock resistance is excell.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidatio.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 170 M RAPID Dense Vibrating Refractory Castable Description: Vibron 170 M Rapid is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sla.. |