Mechanical Properties Metric English Comments
Compressive Strength 112 MPa

@Strain 5 %
16200 psi

@Strain 5 %
ISO 604
Quadrant EPP Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data)
Compared with virgin PA 66, this 30 % glass fibre reinforced and heat stabilised nylon grade offers increased strength, stiffness, creep resistance and dimensional stability whilst retaining an exce..