Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.0700 - 0.110 MPa @Strain 40.0 % |
10.2 - 16.0 psi @Strain 40.0 % |
BS4443 Part 1 Method 5B |
P & P Technology Silicone Sponge The thermal stability of silicone rubber is probably its most important asset. Components made from these rubbers are affected only to a small extent by extremes of temperature, ranging from –90°C.. |