Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-110N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 500 °C, Time 10800 sec |
711 - 1420 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-110N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-120N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 500 °C, Time 10800 sec |
711 - 1420 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-120N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 1000 °C, Time 10800 sec |
711 - 1420 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-120N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-135N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 500 °C, Time 10800 sec |
711 - 1420 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-135N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 1000 °C, Time 10800 sec |
711 - 1420 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-135N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT135S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PT-170 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PTA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PTA-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PTF-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 1350 °C, Time 10800 sec |
711 - 1420 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PAC-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 1500 °C, Time 10800 sec |
711 - 1420 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PAC-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |