Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 127.5 MPa @Strain 10.0 % |
18490 psi @Strain 10.0 % |
ASTM D695 |
Daelim H&L Plavis-MS CM MoS2 Filled Aromatic Polyimide Bearing Compression Molded. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the .. |
|||
Compressive Strength | 127.5 MPa @Strain 10.0 % |
18490 psi @Strain 10.0 % |
ASTM D695 |
Daelim H&L Plavis-MS DF MoS2 Filled Aromatic Polyimide Bearing Direct Formed. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the criti.. |
|||
Compressive Strength | 127.5 MPa @Strain 10.0 % |
18490 psi @Strain 10.0 % |
ASTM D695 |
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po.. |
|||
Compressive Strength | 127.5 MPa @Strain 10.0 % |
18490 psi @Strain 10.0 % |
ASTM D695 |
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing Isostatically Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS .. |