Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 119.7 MPa @Temperature 22.8 °C |
17360 psi @Temperature 73.0 °F |
JIS K7208 |
Mitsui AURUM® PL450C Polyimide
(discontinued **) AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU.. |