Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 117000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 807 MPa

@Temperature 23.9 °C
117000 psi

@Temperature 75.0 °F
Dry, 365° Oven Cured; SACMA 1R-94
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 12K PW HTS Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Compressive Strength 807 MPa

@Temperature 21.1 °C
117000 psi

@Temperature 70.0 °F
Dry
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ Astroquartz 4581 Fabric
MVK-14 Polyimide Astroquartz and S2 glass prepregs are an affordable, easy-to-process material for high-temperature radome and antenna applications. MVK-14 is a non-MDA alternative to BMI, cyanate e..
Copyright © lookpolymers.com All Rights Reserved