Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 76.0 MPa @Strain 5 % |
11000 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Acetron® MD POM-C + metal detectable additive, extruded (ISO Data) Metal detectable POM-C grade High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stabilit.. |
|||
Compressive Strength | 76.0 MPa @Strain 2 % |
11000 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Semitron® ESd 410C PEI, static dissipative, extruded (ISO Data) Having an excellent mechanical performance up to 210 °C, Semitron ESd 410C provides ESd-solutions at higher temperatures. Additionally, Semitron ESd 410C exhibits excellent dimensional stability (l.. |
|||
Compressive Strength | 75.5 MPa @Temperature 110 °C, Time 86400 sec |
11000 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HSC-16SF-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 75.8 MPa @Strain 10.0 % |
11000 psi @Strain 10.0 % |
ASTM D695 |
Ensinger DELRIN® AF DE588 Acetal Homopolymer, 20% PTFE filled (POM) DELRIN® AF DE588 is a 20% PTFE filled homopolymer acetal that is fully tested and certified for use by the United States Navy. The resin is manufactured by DuPont and is used extensively in a varie.. |