Polymer Property : Compressive Strength = 107000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 738 MPa

@Temperature 82.2 °C
107000 psi

@Temperature 180 °F
Wet; Vacuum/Oven Cured; SACMA 1-94
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...