Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 104.00 MPa @Temperature 1200 °C |
15084 psi @Temperature 2190 °F |
after Firing; ASTM C-349 |
Stellar Canada CERAMITE® BKR-F Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |