Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1.80 MPa @Strain 0.200 %, Temperature 150 °C |
261 psi @Strain 0.200 %, Temperature 302 °F |
ASTM D695 |
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures.. |
|||
Compressive Strength | 1.80 MPa @Strain 0.200 %, Temperature 150 °C |
261 psi @Strain 0.200 %, Temperature 302 °F |
ASTM D695 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |
|||
Compressive Strength | 1.80 MPa @Strain 0.200 %, Temperature 150 °C |
261 psi @Strain 0.200 %, Temperature 302 °F |
ASTM D695 |
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures.. |
|||
Compressive Strength | 1.80 MPa @Strain 0.200 %, Temperature 150 °C |
261 psi @Strain 0.200 %, Temperature 302 °F |
ASTM D695 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |