Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.140 MPa @Strain 10.0 % |
20.3 psi @Strain 10.0 % |
DIN-EN 826 |
BASF E-por® 0.03 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |