Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.0117 MPa @Strain 25.0 % |
1.70 psi @Strain 25.0 % |
|
Northstar Polymers MPS-F06B Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and.. |