Polymer Property : Tensile Modulus = 9600 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 66.2 GPa

@Temperature 23.9 °C
9600 ksi

@Temperature 75.0 °F
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS T300 Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Tensile Modulus 66.2 GPa

@Temperature 19.4 °C
9600 ksi

@Temperature 67.0 °F
CTD, 0° Direction; SACMA SRM 4R-94
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric
MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties ..
Tensile Modulus 66.2 GPa

@Temperature 195 °C
9600 ksi

@Temperature 383 °F
0°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber
Information provided by HexCel
Tensile Modulus 66.2 GPa

@Temperature -67.0 °C
9600 ksi

@Temperature -88.6 °F
90°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber
Information provided by HexCel