Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.15 GPa @Temperature 120 °C |
892 ksi @Temperature 248 °F |
|
LATI Lapex A G/20 PES, 20% Glass Fiber Reinforced Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |