Mechanical Properties Metric English Comments
Tensile Modulus 3.85 GPa

@Temperature 60.0 °C
558 ksi

@Temperature 140 °F
LATI Lapex R G/10 PPSU, 10% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..