Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 29.0 GPa @Temperature 23.0 °C |
4210 ksi @Temperature 73.4 °F |
|
LATI Latamid 66 H2 K/50 PA 66, 50% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Tensile Modulus | 29.0 GPa @Temperature 250 °C |
4210 ksi @Temperature 482 °F |
ISO 527-1 |
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex.. |