Mechanical Properties Metric English Comments
Tensile Modulus 39.0 GPa

@Temperature 90.0 °C
5660 ksi

@Temperature 194 °F
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..