Mechanical Properties Metric English Comments
Tensile Modulus 24.8 GPa

@Temperature 21.1 °C
3600 ksi

@Temperature 70.0 °F
0° Direction, Dry; ASTM D638
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 4581 Quartz
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Tensile Modulus 24.8 GPa

@Temperature 82.2 °C
3600 ksi

@Temperature 180 °F
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Tensile Modulus 24.8 GPa

@Temperature 23.9 °C
3600 ksi

@Temperature 75.0 °F
0° Direction, Dry; Autoclave, 50 psi, 90min; ASTM D638
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring ..
Tensile Modulus 24.8 GPa

@Temperature 23.9 °C
3600 ksi

@Temperature 75.0 °F
0° Direction, Wet (2 hour water boil); ASTM D638 Type 1
Park Electrochemical Nelcote® P-650R Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650R is a non-styrenated/low VOC polyester resin system that has been designed for optical clarity. P-650 exhibits good mechanical properties up to 250°F.Key Features and Benefits:Non-s..
Tensile Modulus 24.8 GPa

@Temperature 23.9 °C
3600 ksi

@Temperature 75.0 °F
Dry; ASTM D638
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4503 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Tensile Modulus 24.8 GPa

@Temperature 204 °C
3600 ksi

@Temperature 400 °F
Dry; ASTM D638
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Tensile Modulus 24.8 GPa

@Temperature 177 °C
3600 ksi

@Temperature 351 °F
Hexcel® HexPly® F650 Bismaleimide Resin with Quartz 581 fabric reinforcement
Laminate Physicals: 55.4% Fiber volume, 31.4% Resin content, 0.7% Voids, 1.78% gm.cc Specific gravityInformation provided by HexCel