Polymer Property : Tensile Modulus = 281 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.94 GPa

@Temperature 23.0 °C
281 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® FG133F1 NC010 Nylon 66  (Unverified Data**)
Zytel® FG133F1 NC010 is a nucleated PA 66. It has been developed for consideration into applications such as parts for the food industry.Information provided by DuPont