Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 26.5 GPa @Temperature 90.0 °C |
3840 ksi @Temperature 194 °F |
|
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 26.5 GPa @Temperature 24.0 °C |
3840 ksi @Temperature 75.2 °F |
Dry |
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140Information provided by HexCel |