Polymer Property : Tensile Modulus = 23.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 23.0 GPa

@Temperature 23.0 °C
3340 ksi

@Temperature 73.4 °F
LATI Larton GCE/650 PPS, Glass/Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Modulus 23.0 GPa

@Temperature 60.0 °C
3340 ksi

@Temperature 140 °F
LATI Latamid 66 H2 K/40 PA 66, 40% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Modulus 23.0 GPa

@Temperature 23.0 °C
3340 ksi

@Temperature 73.4 °F
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 23.0 GPa

@Temperature 23.0 °C
3340 ksi

@Temperature 73.4 °F
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced
High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio..