Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 22.0 GPa @Temperature 60.0 °C |
3190 ksi @Temperature 140 °F |
|
LATI Larton GCE/650 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Tensile Modulus | 22.0 GPa @Temperature 23.0 °C |
3190 ksi @Temperature 73.4 °F |
|
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &.. |
|||
Tensile Modulus | 22.0 GPa @Temperature 120 °C |
3190 ksi @Temperature 248 °F |
|
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Tensile Modulus | 22.0 GPa @Temperature 60.0 °C |
3190 ksi @Temperature 140 °F |
|
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Modulus | 22.0 GPa @Temperature 120 °C |
3190 ksi @Temperature 248 °F |
|
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 22.0 GPa @Temperature 150 °C |
3190 ksi @Temperature 302 °F |
|
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Tensile Modulus | 22.0 GPa @Temperature 71.0 °C |
3190 ksi @Temperature 160 °F |
Dry |
Hexcel® HexPly® F522 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F522; Fiber: 75-1/0Information provided by HexCel |
|||
Tensile Modulus | >= 22.0 GPa @Temperature 50.0 °C |
>= 3190 ksi @Temperature 122 °F |
ISO 527-2 |
BASF Ultrason® E 2010 C6 30% Carbon Filled Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu.. |