Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.76 GPa @Temperature 23.9 °C |
400 ksi @Temperature 75.0 °F |
±45° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® F-562 Phenolic Prepreg, C2 Carbonized Rayon Reinforced Nelcote® F-562 is an elastomer modified phenolic resin used in the manufacture of intermediate temperature ablative rocket nozzles, heat shields and combustion chambers in highly oxidative environm.. |
|||
Tensile Modulus | >= 2.76 GPa @Temperature 23.9 °C |
>= 400 ksi @Temperature 75.0 °F |
|
Master Bond EP112LS Two part, heat curing epoxy for potting, encapsulation, coating, sealing and impregnation Master Bond EP112LS is a low viscosity two component epoxy resin system for potting, encapsulation, sealing, coating and impregnation. The mix ratio is an easy to use 100:80 by weight. EP112LS offer.. |