Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 128 GPa @Temperature 82.2 °C |
18600 ksi @Temperature 180 °F |
0° Direction, Wet; Vacuum/Oven Cured; ASTM D3039-95 |