Polymer Property : Tensile Modulus = 1810 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 12.5 GPa

@Temperature 90.0 °C
1810 ksi

@Temperature 194 °F
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 12.5 GPa

@Temperature 23.0 °C
1810 ksi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Modulus 12.5 GPa

@Temperature 90.0 °C
1810 ksi

@Temperature 194 °F
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced
Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle..
Tensile Modulus 12.5 GPa

@Temperature 60.0 °C
1810 ksi

@Temperature 140 °F
LATI Latamid 6 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Modulus 12.5 GPa

@Temperature 23.0 °C
1810 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 12.5 GPa

@Temperature 23.0 °C
1810 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Rynite® 940 BK505 PET  (Unverified Data**)
Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers