Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.130 GPa @Temperature 100 °C |
18.9 ksi @Temperature 212 °F |
1 mm/min; ISO 527-2 |
Solvay Specialty Polymers Polidan® TUX 100 Polyethylene, Crosslinked (XLPE) Polidan® TUX 100 is a high density crosslinkable polyethylene compound manufactured according to the Sioplas® process. It has been developed for the production of crosslinked pipes in a wide r.. |