Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 170 GPa @Temperature 121 °C |
24600 ksi @Temperature 250 °F |
0° Direction, Wet, 365° Autoclave Cured; ASTM D3039 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, IM7 Unitape Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |