Polymer Property : Tensile Modulus = 159 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 159 GPa

@Temperature 25.0 °C
23100 ksi

@Temperature 77.0 °F
0°, Dry
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber
Information provided by HexCel