Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 90.3 GPa @Temperature 23.0 °C |
13100 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® F515 Epoxy Resin, BXX120 Carbon Tape Information provided by HexCel |
|||
Tensile Modulus | 90.0 GPa @Temperature 1000 °C |
13100 ksi @Temperature 1830 °F |
|
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |