Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.60 GPa @Temperature 120 °C |
1100 ksi @Temperature 248 °F |
|
LATI Latamid 6 H2 G/55 PA 6, 55% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Tensile Modulus | 7.60 GPa @Temperature 120 °C |
1100 ksi @Temperature 248 °F |
|
LATI Larton CE/60 PPS, 60% Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; .. |
|||
Tensile Modulus | 7.60 GPa @Temperature 23.0 °C |
1100 ksi @Temperature 73.4 °F |
90° |
Hexcel® HexPly® 954-6 Curing Cyanate Resin, M40J Fiber Information provided by HexCel |
|||
Tensile Modulus | 7.60 GPa @Temperature 23.0 °C |
1100 ksi @Temperature 73.4 °F |
90º, Conditioning: 23°C; ASTM D3039 |
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg M46J Fibre 1947 - 38% resin weight with M46J 52.5% fiber volumeInformation provided by HexCel |
|||
Tensile Modulus | 7.59 GPa @Temperature 93.0 °C |
1100 ksi @Temperature 199 °F |
ASTM D638 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |