Polymer Property : Tensile Modulus = 10000 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 68.9 GPa

@Temperature 195 °C
10000 ksi

@Temperature 383 °F
0°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber
Information provided by HexCel