Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.6 GPa @Temperature 120 °C |
1540 ksi @Temperature 248 °F |
|
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |