Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.234 GPa @Temperature -40.0 °C |
1484.3 ksi @Temperature -40.0 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66
(Unverified Data**) Zytel® 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was developed for applications requiring strength, stiffness and im.. |