Mechanical Properties Metric English Comments
Tensile Modulus 0.370 GPa

@Temperature 80.0 °C
53.7 ksi

@Temperature 176 °F
ISO Data
BASF Ultramid® 8253 HS PA6 (Conditioned)
Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased..